Butyl reclaimed rubber physical test item quality indicators
Sulfide
Time temperature of 160 degrees
It takes about 40 minutes
1 water (80 ),% ≤ 0.50
2 Ash,% ≤ 8.00
3, acetone extract,% ≤ 10.00
4 pull stretch strength MPa ≥ 8.50
Long stretch rate of 5 break,% ≥ 550
6 Density g/cm3 ≤ 1.20
7 Mooney viscosity ML [(1 +4) 100 ] 40