Place of Origin
Fujian, China
Application
Industrial Ceramic
Processing Service
Welding, Cutting, Moulding, CNC
Material
Hot Pressed Boron Nitride/HPBN
Compressive Strength
100 MPa
Thermal Conductivity
15 W/m.k
Thermal Expansion Coefficient
1.5x10(^-6)/K
Volume Resistivity
>10(^14) Ω.cm
Max Operation Temperature
2100 C