Elastic Nylon Thread | Gloves, Crochet, Hand Knitting, Knitting | - Tensile strength: 120 N/tex (ASTM D885-21) - Elongation: 300% recovery (ASTM D638) - Chemical resistance: Resists 50+ chemicals (ASTM D543, 30min) - Eco-friendly: Biodegradable in 6 months (OK Compost INDUSTRIAL) | ▲▲▲ Superior elasticity for stretch applications ▲▲ High durability ▲ Low shrinkage | Higher cost than cotton/polyester Requires specific care to avoid UV damage |
Polyester Thread | General Sewing, Upholstery, Industrial | - Tensile strength: 100 N/tex (ASTM D2256) - Shrinkage: <5% after boiling (ISO 599-1) - Mildew resistance: ASTM D3486 compliant | ▲▲ Cost-effective ▲ Resists abrasion and chemicals | Low elasticity Not biodegradable Prone to static buildup |
Cotton Thread | Clothing, Quilting, Embroidery | - Tensile strength: 80 N/tex (ASTM D2256) - Softness: ISO 13934-1 compliant - Biodegradability: 100% natural fiber | ▲▲ Natural feel and breathability ▲ Easy to dye | Low chemical resistance Prone to abrasion and shrinkage |
Spandex Thread | Activewear, Swimwear, Stretch Fabrics | - Elongation: 500% (ASTM D638) - Flexibility: ISO 13934-2 compliant - UV resistance: ASTM G154, 500 hours | ▲▲▲ Extreme stretch recovery ▲ Lightweight | ▲▲ Lower durability over time UV degradation without additives |
Silk Thread | Luxury Garments, Decorative Stitching | - Luster: ASTM D1234-17 compliant - Tensile strength: 80 N/tex (ASTM D885) - Smoothness: ISO 13934-3 compliant | ▲▲▲ Aesthetic appeal ▲ Lightweight and hypoallergenic | High cost Brittle when wet Low abrasion resistance |
Wool Thread | Knitting, Winter Apparel, Upholstery | - Insulation: EN 3109-1 compliant - Elasticity: 200% recovery (ASTM D638) - Flame resistance: NFPA 701 compliant | ▲▲ Natural thermal insulation ▲ Resists static | Prone to moth damage High shrinkage without treatment Expensive |