Injection Molding Grade | Automotive parts, medical devices | High Temperature Resistance: Industry Standard: 200°C Our Base: 240°C▲ Our Advanced: 260°C▲▲ (ASTM D648) | Our Advanced grade withstands extreme heat (e.g., engine components), reducing thermal deformation risks. | Advanced grade may require specialized equipment for processing. |
Extrusion Grade | Pipes, profiles, blown films | High Flow: Industry Standard: 10 g/10min Our Base: 15 g/10min▲ Our Advanced: 20 g/10min▲▲ (ISO 1133) | Faster extrusion speeds with Our Advanced reduce production time by 30%. | Lower mechanical strength in Base/Advanced grades may limit load-bearing applications. |
Blow Molding Grade | Bottles, containers, packaging | Impact Resistance: Industry Standard: 200 J/m Our Base: 250 J/m▲ Our Advanced: 300 J/m▲▲ (ASTM D256) | Advanced grade prevents cracking in thin-walled bottles during handling. | Higher material cost for Advanced may affect cost-sensitive packaging. |
Rotational Molding Grade | Large hollow products (toys, tanks) | Hydrolysis Resistance: Industry Standard: 500 hours Our Base: 700 hours▲ Our Advanced: 1000 hours▲▲ (ASTM D1693) | Advanced grade maintains integrity in humid environments (e.g., water tanks). | Longer curing times for Advanced may slow production. |
Coating Grade | Pipes, wires, automotive coatings | UV Resistance: Industry Standard: 500 hours Our Base: 700 hours▲ Our Advanced: 1000 hours▲▲ (ASTM G154) | Advanced coating resists UV degradation for outdoor applications (e.g., solar panels). | Requires thicker coatings, increasing material usage. |
Foaming Grade | Insulation, packaging, automotive parts | Thermal Insulation: Industry Standard: 0.15 W/m·K Our Base: 0.12▲ Our Advanced: 0.09▲▲ (ASTM C518) | Advanced grade reduces heat transfer by 40%, ideal for refrigeration units. | Foaming process may introduce voids affecting structural integrity. |